A parametric study on tribological and mechanical performance of dental acrylic (PMMA)-coated FDM PETG
2026 (English)In: AIMS Materials Science, E-ISSN 2372-0484, Vol. 13, no 4, p. 832-856Article in journal (Refereed) Published
Abstract [en]
Fused deposition modeling (FDM) fabricated polyethylene terephthalate glycol (PETG) may have a corrugated surface and voids between the layers, which can restrict performance in sliding contact. In this study, we investigated a low-cost surface engineering process where the tribologically challenging PETG substrate was structurally selected and the protective coating was the self-curing dental polymethyl methacrylate (PMMA). Three levels of each of the four FDM parameters were screened, with three independently printed specimens for each level of the parameter. Three-trial wear indices were analyzed using the original Taguchi smaller-the-better signal-to-noise (S/N) criterion, and factor-level means and sample standard deviations (SDs) were used to summarize the results for tensile strength, Rockwell R hardness (HRR), and inclined-plane static coefficient of friction (COF). The archived measurements were factor-level triplicates as opposed to responses associated with nine simultaneous L9 combinations. Selected PETG specimens were cross-hatched, acetone cleaned, dip-coated, and cured for 48 h. The coating was applied evenly at 0.5 mm on each face, increasing each reduced-section dimension by 1.0 mm in total. The coated condition had a mean maximum load 24.1% greater. Using condition-specific outer-section areas, the calculated tensile strength was 6.9% lower (27.15 +/- 0.48 versus 25.29 +/- 0.46 MPa), whereas the calculated tensile modulus was 13.8% higher (6.20 +/- 0.25 versus 7.05 +/- 0.19 MPa). Mean hardness was 44.2% higher (60.0 +/- 0.8 versus 86.5 +/- 0.7 HRR). The apparent PETG-equivalent wear index, calculated using a common PETG-density normalization due to the inability to separate the lost PMMA and PETG phases, was 50.0% lower ((27.77 +/- 3.97) & times; 10-3 versus (13.88 +/- 1.98) & times; 10-3 mm3 N-1 m-1). Static COF was 2.0% lower (0.1643 +/- 0.0005 versus 0.1611 +/- 0.0005), although the absolute change was small. The scanning electron microscopy (SEM) images revealed a more continuous coated surface and no large-scale delamination following the short duration abrasive test.
Place, publisher, year, edition, pages
American Institute of Mathematical Sciences, 2026. Vol. 13, no 4, p. 832-856
Keywords [en]
FDM, PETG, PMMA coating, tribology, abrasive wear, surface engineering, additive manufacturing
National Category
Materials Engineering
Identifiers
URN: urn:nbn:se:oru:diva-131434DOI: 10.3934/matersci.2026039ISI: 001875144200001OAI: oai:DiVA.org:oru-131434DiVA, id: diva2:2103922
2026-09-222026-09-222026-09-22Bibliographically approved